PRO-SET® Special Order Formulations
PRO-SET® Special Order Epoxies are designed for very specific applications or manufacturing processes.
					STANDARD INFUSION SYSTEMS
PRO-SET® Special Order Epoxies are designed for very specific applications or manufacturing processes. Each system has been formulated to meet the demands of a specific customer’s application when the volume warrants tailored formulation. Even though developed for a well-defined application, as the composite industry grows and changes, new users often find uses for these Special Order formulations.
A four-digit number preceded by the letter M identifies the resins and hardeners in the Special Order group. All resin numbers begin with the number 1 and the hardeners begin with the number 2.
Expanding Epoxy Foam
Expand in-place foam that, when mixed, creates an in-situ closed cell epoxy foam with very uniform cell size.
PRO-SET® M1002 toughened laminating resin is formulated for high load or high peel applications and situations where the bond line area is less than optimum. Examples are carbon fibre skins on honeycomb core material or tabbing with carbon onto cured carbon skinned panels and structures.
Fire Retardant Laminating Epoxy
The PRO-SET® Fire Retardant Laminating System is a low-viscosity system containing high phosphorous levels. This feature helps reduce flame spread and smoke generation in a composite laminate compared to a standard epoxy system. Proper post-curing provides excellent temperature stability and enhances the cosmetic appearance of the final part.
Epoxy Gelcoats
PRO-SET® offers in mould epoxy gelcoats and three PRO-SET hardeners that can be used with the gelcoat resins.
Phenol-free PRO-SET M2048 and M2049 Hardeners greatly improve the colour stability and durability of gelcoat systems, but UV exposure will still cause discolouration.
Custom Formulations
We offer custom formulated resin and hardener systems tailored to your specific process and performance needs. We work closely with you throughout the development process to ensure your custom formulation meets your exact requirements. Contact us for further details.
Expanding Epoxy Foam
- PRO-SET M1034 with M2037 Expanding Epoxy Foam
 
Super Toughened Laminating Epoxy
- PRO-SET M1002 with LAM-224 Fast Cure Toughened Laminating Epoxy
 - PRO-SET M1002 with LAM-226 Medium Cure Toughened Laminating Epoxy
 - PRO-SET M1002 with LAM-229 Slow Cure Toughened Laminating Epoxy
 - PRO-SET M1002 with LAM-237 Extra Slow Cure Toughened Laminating Epoxy
 
Fire Retardant Laminating Epoxy
- PRO-SET M1048 with LAM-237 Fire Retardant Laminating Epoxy
 
Epoxy Gelcoats
- M1044 Translucent Gelcoat
 - M1045 White Gelcoat
 - M1046 Black Gelcoat
 - M2015 Fast
 - M2048 Medium
 - M2049 Slow
 
Gelcoats
Use with M2015, M2048, M2049 Custom Hardeners
| Product Code | Description | Size | 
|---|---|---|
| M1044 | Translucent Gelcoat | 2.5kg | 
| M1044 | Translucent Gelcoat | 5kg | 
| M1044 | Translucent Gelcoat | 20kg | 
| M1045 | White Gelcoat | 2.5kg | 
| M1045 | White Gelcoat | 5kg | 
| M1045 | White Gelcoat | 20kg | 
| M1046 | Black Gelcoat | 2.5kg | 
| M1046 | Black Gelcoat | 5kg | 
| M1046 | Black Gelcoat | 20kg | 
                    Our Experienced Team is Available to Help